The aim of the current work is to present a new route to synthesise carbonateapatite with low cristallinity and carbonate content in the range of biological apatites. Mechanical milling has been employed for this preparation and the influence of the different conditions on the final material characteristics has been studied. A higher time of grinding is required under a CO_2 atmosphere (210 hours) than under air (135 hours). However, in the sample obtained in air, some of the starting CaCO_3 still remains.
机译:当前工作的目的是提出一种合成生物磷灰石范围内低结晶度和低碳酸盐含量的碳酸盐磷灰石的新途径。机械研磨已用于该制备,并且已经研究了不同条件对最终材料特性的影响。与在空气中(135小时)相比,在CO_2气氛(210小时)中需要更长的研磨时间。但是,在空气中获得的样品中,仍然保留了一些起始CaCO_3。