A recommended practice for design of titanium risers is currently being developed as part of Det Norske Veritas' series of standards and recommended practices for offshore structures. A recommendation is given herein for characteristic S-N curves for use in design of titanium risers against fatigue failure. As a basis for this recommendation, a set of statistical analyses of available fatigue test data have been carried out. Separate analyses have been carried out for base material and welds. The analysis results have been interpreted with respect to mean S-N curves as well as 97.7% lower tolerance bounds with 95% confidence. Characteristic S-N curves for base material and welds, which are not non-conservative with respect to these tolerance bounds, have been proposed. The paper presents the assumptions, the test data, the statistical analyses and their results, and the proposed characteristic S-N curves. The areas of application of the proposed curves are discussed with a particular view to stress range interval, material grade, weld position, temperature, and defect size.
机译:目前,作为Det Norske Veritas系列标准和海上结构建议做法的一部分,正在开发钛冒口设计的建议做法。本文给出了用于设计钛立管抗疲劳破坏的特征S-N曲线的建议。作为此建议的基础,已对可用的疲劳测试数据进行了一组统计分析。已经对基础材料和焊缝进行了单独的分析。分析结果已针对平均S-N曲线以及具有97%置信度的97.7%较低的公差范围进行了解释。已经提出了针对这些公差范围并非保守的基础材料和焊缝的特征S-N曲线。本文介绍了假设,测试数据,统计分析及其结果以及拟议的特征S-N曲线。讨论了拟议曲线的应用领域,并特别讨论了应力范围间隔,材料等级,焊接位置,温度和缺陷尺寸。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号